Polyester-based Thermoplastic Polyurethane
Properties | Key | NORM | Value | Unit |
---|---|---|---|---|
Hardness (after 3 sec.) | M | ASTM D 2240 | 55 | Shore A |
Density | M | ASTM D 792 | 1.13 | g/cm³ |
Tensile strength | E | ASTM D 412 | 2100 | psi |
Elongation @ break | E | ASTM D 412 | 610 | % |
Tensile stress @ 100% elongation | E | ASTM D 412 | 250 | psi |
Tensile stress @ 300% elongation | E | ASTM D 412 | 400 | psi |
Tensile set @ 200% Elongation | E | ASTM D 412 | 5 | % |
Tear strength | E | ASTM D 624 | 220 | pli |
Softening range low | E | Huntsman TMA | 105 | °C |
Softening range high | E | Huntsman TMA | 135 | °C |
Glass transition temperature (DSC) | ASTM D 3418 | -42 | °C |
M = Injection moulded parts to meet DIN & ASTM requirements. Parts tempered for 20 hrs @ 100 °C prior to testing
E = Extruded film cut to ASTM requirements. Parts at room temperature aged prior to testing.
Melt Volume Rate [160°C / 8,7kg] ISO 1133-1 = 20 cm³/10min
Processing Parameter: | Extrusion |
Temperature Profile | °C |
Feed Zone: | 25 - 40 |
Barrel: | 160 - 170 |
Die Head: | 165 - 175 |
Nozzle: | 160 - 170 |
Processing Parameter: | Calendering |
Temperature Profile | °C |
Front Roll: | 110 - 120 |
Rear Roll: | 110 - 120 |